Woule kabòn ki ba Q235 Q345 Q355 Ss400 S235jr S355jrcold woule asye bobin

Jan 09, 2026 Kite yon mesaj

K: Ki konpozisyon chimik prensipal yo (fraksyon mas, %) bobin Q355?

A: C Mwens pase oswa egal a 0.20, Si Mwens pase oswa egal a 0.55, Mn Mwens pase oswa egal a 1.60, P Mwens pase oswa egal a 0.035, S Mwens pase oswa egal a 0.035; ka gen ladan eleman microalloying tankou Nb mwens pase oswa egal a 0.06, V mwens pase oswa egal a 0.12, Ti mwens pase oswa egal a 0.20, ki fè yo espesyalman ajiste selon klas la ak epesè.

K: Ki enfliyans epesè sou fòs sede bobin Q355?

A: Mwens pase oswa egal a 16mm Pi gran pase oswa egal a 355MPa; 16-40mm Pi gran pase oswa egal a 345MPa; 40-63mm Pi gran pase oswa egal a 335MPa; 63-80mm Pi gran pase oswa egal a 325MPa; 80-100mm Pi gran pase oswa egal a 315MPa; 100-150mm Pi gran pase oswa egal a 305MPa.

K: Ki sa ki ranje fòs rupture nan bobin Q355?

A: 470-630MPa, yon ti kras varye ak epesè ak pwosesis woule.

K: Ki egzijans elongasyon bobin Q355 la?

A: Klas A/B Pi gran pase oswa egal a 21%; Klas C/D/E Pi gran pase oswa egal a 22%, asire fòmabilite ak severite.

K: Ki kondisyon ki ba -tanperati enpak bobin Q355D?

A: Enèji enpak longitudinal V-dan nan -20 degre pi gran pase oswa egal a 34J, apwopriye pou estrikti deyò nan rejyon frèt.